Aloi Timah Indium Bismut

Alloy Ratio In51Bi32.5Sn16.5 or as required.
Ketumpatan 7.88g/cm3
Takat Lebur 60°C
Thermal expansion coefficient 22
Thermal Conductivity 25W/m/K
Tensile Strength 33.44Mpa