Indium Bismuth Tin Legering

Alloy Ratio In51Bi32.5Sn16.5 or as required.
Massefylde 7.88g/cm3
Smeltepunkt 60°C
Thermal expansion coefficient 22
Termisk ledningsevne 25W/m/K
Tensile Strength 33.44Mpa